Alloy 52

Nominal composition,%

Alloy 

designation

Ni

Cr

Mn

Si

C

Al

Mn

P

S

Fe

Alloy 52

50.5

0.25 max

0.80 max

0.30 max

0.05 max

0.10 max

0.5max

0.025 max

0.025 max

Bal


Availability:
Alloy 52 is available in Sheet, Strip , Plate and Wire.